Substrates |
1K Basecoat. |
||||
Mixing Ratio |
Clear Coat |
Hardener |
Thinner |
||
2 |
1 |
0.2~0.5 | |||
<15℃ |
Clear Coat |
Mating Fast Hardener |
60 Fast Thinner |
||
15-30℃ |
Clear Coat |
Mating Standard Hardener |
61 Standard Thinner |
||
>30℃ |
Clear Coat |
Mating Slow Hardener |
62 Slow Thinner |
||
SprayViscosity |
16-19s to drop off, in 4# viscosity cup at 25°C, |
||||
Pot-Life |
At 25℃ ,4 hours with fast hardener.4 hours with standard hardener or slow hardener. |
||||
Re-Treatment |
There are particles or runs after spray, sand affected area with P2000 sand paper after thorough drying, then polish to solve the problem. |
||||
Spray GunSet Up |
Gravity Feed: 1.2-1.5mm 4-5kg/cm ² Suction Feed: 1.4-1.6mm 4-5kg/cm ² |
||||
SprayTechnology |
Coats&Thickness: 2-3 coats, total 25-35um Flash-Off Time: At 25°C, 5-10 minutes between two coats, Air-Drying Time: Allow 10-15 minutes air drying time before force drying |
||||
Drying Time |
Temperature |
Dust Free |
Tack Free |
Dry to Handle |
Dry to Test |
25°C |
30 minutes |
2 hours |
8 hours |
6 days |
|
70°C |
5 minutes |
10 minutes |
25 minutes |
60 minutes |
|
Shelf Life |
2 years in original sealed can, cool and dry place at 20℃. |
||||
Package |
5L×4 or 2.5L×8 or 5L+2.5L+1L |
Note:
1. At temperature lower than 15°C, air-dry at ambient temperature is not recommended. Better to allow a full bake at 60°C.
2. At ambient temperature higher than 30℃, add appropriate Retarder Solvent into thinner to avoid blushing. For more details, please refer to technical data sheet of Retarder Solvent.
3. The products mixed with hardener should be used up soon and can not be restore for future use; clean equipments immediately with thinner after application, otherwise it is very difficult to be cleaned after dry.